1. All properties are measured at 70°F – 75°+ unless otherwise indicated and all test values from independent certified testing laboratories.
(2. These are nominal values obtained from representative product samples, and are subject to normal manufacturing variances.
3. Average value through the foam cross section.
4. Above 300°F, discoloration and charring will occur, resulting in an increased K-Factor in the discolored area.
5. Frequent and severe thermal cycling can produce dimensional changes significantly greater than those listed here. Special design considerations must be made in systems subject to severe cycling.
6. This numerical flame spread data is not intended to reflect hazards presented by this or any other material under actual fire conditions.